Fading in sublimation printing is a common issue, but it’s often fixable by addressing specific factors in the process. Below is a step-by-step guide to troubleshooting and resolving fading problems when using sublimation paper:
I'm sorry, but it seems that you haven't provided the text you want to be translated. Please provide the text, and I'll be happy to assist you with the translation.
1. Issiqlik Pressi Sozlamalarini Tekshiring
Muammo: Noto'g'ri vaqt, harorat yoki bosim.
Yechimlar
- Harorat: Issiq pressani 180–220°C (356–428°F) ga o'rnating. Juda past = to'liq sublimatsiya emas; juda baland = kuyish.
- Vaqt: Bosish vaqtini 30–60 soniyaga moslang (asosga qarab o'zgaradi). Barqarorlik uchun vaqt o'lchagichdan foydalaning.
- Pressure: Qog'oz va substrat o'rtasida to'liq aloqa o'rnatish uchun mustahkam, bir xil bosim (40–60 psi) qo'llang.
Test: Kichik test bosma amalga oshiring, substratingiz uchun optimal sozlamalarni topish uchun bosqichma-bosqich o'zgartirishlar bilan.
I'm sorry, but it seems that you haven't provided the text you want to be translated. Please provide the text, and I'll be happy to assist you with the translation.
2. Sublimatsiya qog'ozining sifatini tasdiqlang
Muammo: Past sifatli yoki muddati o'tgan qog'oz, noto'g'ri saqlash yoki noto'g'ri tur.
Yechimlar
- Yuqori o'tkazish samaradorligiga ega qog'ozdan foydalaning.
- Qog'ozni salqin, quruq joyda saqlang (namlik qog'ozni egib, siyohni singdirishni kamaytiradi).
- Muddatidan o‘tgan qog‘ozdan foydalanishdan saqlaning.
I'm sorry, but it seems that you haven't provided the text you want me to translate. Please provide the text, and I'll be happy to assist you with the translation.
3. Sublimatsiya siyohini tekshirish
Muammo: Muddati o'tgan siyoh, to'siq bo'lgan bosma boshlar yoki noto'g'ri siyoh turi.
Yechimlar
- Yangi, bo'yoq-sublimatsiya siyohidan foydalaning.
- Printer nozzle'larini muntazam tozalang, to'siqlarning oldini olish uchun (nozzle tekshiruvi o'tkazing).
- Mürekkep kartuşlarının pigmentleri karıştırmak için montajdan önce nazikçe çalkalandığından emin olun.
I'm sorry, but it seems that you haven't provided the text you want translated. Please provide the text, and I'll be happy to assist you with the translation.
4. Substrat Mosligini Baholang
Muammo: Substrat polyesterga boy yoki polimer bilan qoplangan emas.
Yechimlar
- ≥65% poliester matolarni yoki sublimatsiya bilan qoplangan qattiq yuzalarni (kofe ichadigan idishlar, telefon qoplamalari) ishlating.
- Paxta yoki polimer bo'lmagan materiallar uchun avval sublimatsiya püskürtme qoplamasini qo'llang.
I'm sorry, but it seems that you haven't provided the text you want to be translated. Please provide the text, and I'll be happy to assist you with the translation.
5. Namlik ifloslanishini tekshiring
Muammo: Qog'oz, substrat yoki muhitdagi namlik.
Yechimlar
- Substratni namlikni olib tashlash uchun bosishdan oldin 5–10 soniya davomida oldindan qizdiring.
- Sublimatsiya qog'ozini quruq paketlar bilan muhrlangan sumkada saqlang.
- Namli muhitlarda ishlashdan qoching (zarurat bo'lsa, namlikni olib tashlovchi qurilma ishlating).
I'm sorry, but it seems that you haven't provided any text to translate. Please provide the text you would like me to translate into Uzbek.
6. Dizayn Tayyorlashni Moslashtirish
Muammo: Past sifatli san'at asarlari yoki noto'g'ri rang profillari.
Yechimlar
- Oqilona, jonli chop etish uchun 300+ DPI tasvirlardan foydalaning.
- CMYK rejimida dizayn qiling va printeringizni aniq rang moslashuvi uchun kalibrlang.
- Rasmni chop etishdan oldin aks ettiring (mug'lar kabi qattiq substratlar uchun muhim).
I'm sorry, but I cannot assist with that.
7. Issiqlik Pressining Tengligini Tasdiqlang
Muammo: Qiyshiq plita yoki axlat tufayli notekis issiqlik taqsimoti.
Yechimlar
- Issiqlik bosim plitkasini muntazam tozalang (yopishtiruvchi qoldiqlar yoki to'qimalarni olib tashlang).
- Teng bosimni ta'minlash uchun issiqqa chidamli pad yoki silikon varaqdan foydalaning.
- Plitani tekshirib ko'ring va agar shikastlangan bo'lsa, almashtiring.
I'm sorry, but it seems that you haven't provided the text you want to be translated. Please provide the text, and I'll be happy to assist you with the translation.
8. Sinov O'tkazish Texnikasi
Muammo: Erta qoplash, siljish yoki notekis joylashuv.
Yechimlar
- Sublimatsiya qog'ozini substratga issiqqa chidamli lenta bilan mahkamlang.
- Qattiq substratlar uchun bosgandan so'ng (issiq) qog'ozni darhol qopqog'idan olib tashlang yoki matolarni biroz sovutib qo'ying.
- Presslash paytida qog'ozni harakatlantirishdan qoching.
I'm sorry, but it seems that you haven't provided any text to translate. Please provide the text you would like me to translate into Uzbek.
9. Atrof-muhit omillarini ko'rib chiqish
Muammo: Balansning qaynatish nuqtalariga yoki sovuq ish joyiga ta'siri.
Yechimlar
- Yuqori balandliklarda, haroratni biroz oshiring (past qaynoq nuqtalari sababli).
- Ishchi joyning harorati xona haroratida bo'lishini ta'minlang (sovuq yuzalar kondensatsiyaga olib kelishi mumkin).
I'm sorry, but it seems that you haven't provided any text to translate. Please provide the text you'd like me to translate into Uzbek.
10. Himoya varaqalarini tekshiring
Muammo: Eski yoki iflos Teflon varaklari issiqlikni to'sib qo'yadi.
Yechimlar
- Chizilgan yoki dog'langan Teflon varaqalari/qog'ozlarni almashtiring.
- Yaxshi issiqlik taqsimoti uchun yopishmaydigan silikon varaqalardan foydalaning.
I'm sorry, but it seems that you haven't provided the text you want to be translated. Please provide the text, and I'll be happy to assist you with the translation.
Tez Muammo Hal qilish Ro'yxati:  
Belgi
Ehtimoliy Sabab
Tuzatish
So'ndirilgan ranglar
Past harorat/vaqt
Issiqlikni oshirish yoki bosish davomiyligini oshirish
Patchy transfer
Teng bo'lmagan bosim
Bosimni sozlang, plitani tozalang
Suyuq yoki rangsiz
Noto'g'ri substrat/qoplama
Polyester yoki qoplangan bo'shliqlardan foydalaning
Qorong'u rasm
Qog'oz/asiqdagi namlik
Substratni oldindan qizdirish, quruq saqlash
Rang o'zgarishlari
Noto'g'ri printer profili
Printer/ink tizimini qayta kalibrlash
Pro Tip:
Har doim yangi materiallar yoki sozlamalar bilan kichik partiyani sinab ko'ring. Muvaffaqiyatni takrorlash va xatolarni oldini olish uchun o'zgartirishlaringizni hujjatlashtiring. Muammo keltirib chiqarayotgan o'zgaruvchini izolyatsiya qilganingizda, rangning o'chishi ko'pincha oddiy tuzatishdir!